Length-weight relationships of 52 species of fish are presented. Fish were caught during demersal trawl surveys in September-October 1993 and 1994 in northern...
Formation resistivity factor (F) and pore-surface resistivity (... c ) values were determined for three mineralized and nonmineralized rock samples from the...
The electrical conductivity mechanisms have been determined for six mineralized sericite schist specimens cut from a large sample collected from the Gold Lake...
Effective porosity measurements were performed on a suite of 17 samples from the Yellowknife mining district, Northwest Territories. The samples include...
The electrical resistivity characteristics have been determined for five black graphitic shale samples collected from the Astarte River formation, Piling Group...
Spectral induced polarization (spectral-IP) characteristics of pairs of graphite electrodes have been measured to determine the capacitance characteristics of...
Spectral induced polarization measurements have been performed over a frequency range of 1 10 6 Hz on a suite of four mineralized and nonmineralized rock...